ZL102铝合金不同体系阳极氧化工艺和膜层性能研究

  • 戴美洛 ,
  • 秦会斌
展开
  • 杭州电子科技大学 电子信息学院,浙江 杭州 310018
戴美洛(1999-),男,硕士研究生,研究方向:电路与系统,E-mail:hsy_dml@163.com。
秦会斌(1961-),男,教授,研究方向:新型电子器件、抗电磁干扰、分布式储能等,E-mail:qhb@hdu.edu.cn。

收稿日期: 2024-02-27

  网络出版日期: 2025-12-16

基金资助

安徽省重点研究与开发计划项目(202004g01020003)

Study on anodic oxidation process and film properties of ZL102 aluminum alloy in different systems

  • DAI Meiluo ,
  • QIN Huibin
Expand
  • School of Electronics & Information, Hangzhou Dianzi University, Hangzhou Zhejiang 310018, China

Received date: 2024-02-27

  Online published: 2025-12-16

摘要

采用硫酸、硫酸-草酸、硫酸-酒石酸、硫酸-柠檬酸这四种溶液体系,在ZL102铝合金表面制备阳极氧化膜,考察了添加相同摩尔浓度的有机酸对所得膜层性能的影响。采用金相显微镜观察了氧化膜的表面微观形貌,并用细胞计数法得到了孔隙率比例。采用涡流法测量了膜层的厚度,并用金相法验证。通过维氏硬度试验测试了阳极氧化前后ZL102铝合金的力学性能。采用耐电压试验测试了膜层的电学性能。采用导热试验测试了阳极氧化前后的热学性能。结果表明:ZL102铝合金在4种体系中均能获得颜色均一、表面光滑的氧化膜,在硫酸-草酸中形成的阳极氧化膜最厚,可达27.5 μm。添加有机酸能减小孔隙率,并且添加草酸的效果最好。各体系阳极氧化硬度提升程度基本一致,都超过45%。在未封孔的情况下,各体系阳极氧化提升的点耐电压都超过1.5 kV,硫酸-草酸体系最高,可达1.698 kV;直径10 mm单面耐电压都超过0.5 kV,硫酸中最高,可达 0.777 kV。各体系阳极氧化提升的热阻都超过64%,降低了导热性能,但是添加有机酸有助于热阻的降低。综合来看,在硫酸中添加草酸的溶液体系中进行ZL102铝合金的阳极氧化得到的综合性能较优。

本文引用格式

戴美洛 , 秦会斌 . ZL102铝合金不同体系阳极氧化工艺和膜层性能研究[J]. 杭州电子科技大学学报, 2025 , 45(6) : 69 -76 . DOI: 10.13954/j.cnki.hdu.2025.06.008

Abstract

The anodic oxide film was prepared on the surface of ZL102 aluminum alloy with sulfuric acid, sulfuric acid-oxalic acid, sulfuric acid-tartaric acid and sulfuric acid-citric acid. The effect of organic acid with the same molar concentration on the properties of the film was investigated. The surface morphology of the oxide film was observed by metallographic microscope and the porosity ratio was obtained by using cell counting method. The thickness of the film was measured by eddy current method and verified by metallographic method. The mechanical properties of ZL102 aluminum alloy before and after anodizing were tested by Wechsler hardness test. The electrical properties of the film were tested by withstand voltage resistance test. The thermal properties before and after anodic oxidation were tested by thermal conductivity test. The results show that the uniform color and smooth surface oxide films of ZL102 aluminum alloy can be obtained in all of the four systems, and the anodic oxide film formed in sulfuric acid-oxalic acid is the thickest, up to 27.5 μm. The addition of organic acids can reduce the porosity, and oxalic acid achieves the best effect. The anodic oxidation hardness of each system is basically the same, more than 45%. In the case of unsealed holes, the point withstand voltage of anodic oxidation of each system is more than 1.5 kV, and the highest voltage of sulfuric acid-oxalic acid system is up to 1.698 kV. The diameter of 10 mm single-side voltage is more than 0.5 kV, the highest in sulfuric acid, up to 0.777 kV. The anodic oxidation of each system increased the thermal resistance by more than 64%, which reduced the thermal conductivity, but the addition of organic acids helped to reduce the thermal resistance. In summary, the comprehensive properties of ZL102 aluminum alloy were better in the solution system with oxalic acid added to sulfuric acid.

参考文献

[1]罗兵辉, 柏振海, 周华, 等. 几种铸造铝合金的铸造性能、力学性能及耐蚀性[J]. 矿冶工程, 2001(2): 67-68.
[2]WU R Z, QU Z K, ZHANG M L. Reviews on the influences of alloying elements on the microstructure and mechanical properties of Mg-Li base alloys[J]. Reviews on Advanced Materials Science, 2010, 24(1): 35-43.
[3]管仁国, 娄花芬, 黄晖, 等. 铝合金材料发展现状、趋势及展望[J]. 中国工程科学, 2020, 22(5): 68-75.
[4]SERSOUR Z, AMIROUCHE L. Effect of aging and annealing treatments on the microstructural behavior of some Al-Si based alloys[J]. Applied Mechanics and Materials, 2015, 775: 152-159.
[5]林枫, 陆文兴, 吴孟武. 热处理对压铸铝合金ZL102力学及导热性能的影响[J]. 铸造, 2022, 71(6): 683-688.
[6]金星, 高立新, 张大全. Al-Si合金腐蚀与防护的研究进展[J]. 全面腐蚀控制, 2010, 24(9): 12-16.
[7]郑弃非, 孙霜青, 温军国. 铝及铝合金在我国的大气腐蚀及其影响因素分析[J]. 腐蚀与防护, 2009, 30(6): 359-363.
[8]JIN G, LI S, LOU C S. The anode oxidation technics and the characteristics of the films of ZL101A Al-Si alloy[J]. Advanced Materials Research, 2014, 893: 566-569.
[9]SULLIVAN J P O, WOOD G C. The morphology and mechanism of formation of porous anodic films on aluminium[C]//Proceedings of the Royal Society A: Mathematical, Physical and Engineering Sciences (PRSA). 1970. London, England, UK. The Royal Society, 1970, 317(1531): 511-543.
[10]廖重重, 陈岁元. 铝阳极氧化膜及生长机理的研究进展[J]. 辽宁化工, 2012, 41(7): 699-701.
[11]王雨辰. 铝合金硫酸阳极氧化槽液的质量控制[J]. 科技创新与生产力, 2023, 44(8): 91-93.
[12]王英君, 刘洪雷, 王国军, 等. 新型高强稀土Al-Zn-Mg-Cu-Sc铝合金的阳极氧化及其抗腐蚀性能研究[J]. 中国腐蚀与防护学报, 2020, 40(2): 131-138.
[13]高崇, 江钟宇, 赵丕植, 等. 电流密度对5252铝合金阳极氧化膜性能的影响[J]. 电镀与环保, 2020, 40(3): 63-66.
[14]薛莹. 铝合金阳极氧化封孔工艺的探析[J]. 冶金与材料, 2021, 41(6): 129-130.
[15]张策, 张德忠, 潘学著, 等. 铝及铝合金阳极氧化膜封孔技术机理、应用及研究进展[J]. 电镀与涂饰, 2022, 41(18): 1305-1312.
[16]库尔班江·乌丝曼, 戴晓业, 史琳. 相变材料对储热系统换热速率的影响[J]. 东北大学学报(自然科学版), 2023, 44(9): 1292-1297.