The anodic oxide film was prepared on the surface of ZL102 aluminum alloy with sulfuric acid, sulfuric acid-oxalic acid, sulfuric acid-tartaric acid and sulfuric acid-citric acid. The effect of organic acid with the same molar concentration on the properties of the film was investigated. The surface morphology of the oxide film was observed by metallographic microscope and the porosity ratio was obtained by using cell counting method. The thickness of the film was measured by eddy current method and verified by metallographic method. The mechanical properties of ZL102 aluminum alloy before and after anodizing were tested by Wechsler hardness test. The electrical properties of the film were tested by withstand voltage resistance test. The thermal properties before and after anodic oxidation were tested by thermal conductivity test. The results show that the uniform color and smooth surface oxide films of ZL102 aluminum alloy can be obtained in all of the four systems, and the anodic oxide film formed in sulfuric acid-oxalic acid is the thickest, up to 27.5 μm. The addition of organic acids can reduce the porosity, and oxalic acid achieves the best effect. The anodic oxidation hardness of each system is basically the same, more than 45%. In the case of unsealed holes, the point withstand voltage of anodic oxidation of each system is more than 1.5 kV, and the highest voltage of sulfuric acid-oxalic acid system is up to 1.698 kV. The diameter of 10 mm single-side voltage is more than 0.5 kV, the highest in sulfuric acid, up to 0.777 kV. The anodic oxidation of each system increased the thermal resistance by more than 64%, which reduced the thermal conductivity, but the addition of organic acids helped to reduce the thermal resistance. In summary, the comprehensive properties of ZL102 aluminum alloy were better in the solution system with oxalic acid added to sulfuric acid.
DAI Meiluo
,
QIN Huibin
. Study on anodic oxidation process and film properties of ZL102 aluminum alloy in different systems[J]. Journal of Hangzhou Dianzi University, 2025
, 45(6)
: 69
-76
.
DOI: 10.13954/j.cnki.hdu.2025.06.008
[1]罗兵辉, 柏振海, 周华, 等. 几种铸造铝合金的铸造性能、力学性能及耐蚀性[J]. 矿冶工程, 2001(2): 67-68.
[2]WU R Z, QU Z K, ZHANG M L. Reviews on the influences of alloying elements on the microstructure and mechanical properties of Mg-Li base alloys[J]. Reviews on Advanced Materials Science, 2010, 24(1): 35-43.
[3]管仁国, 娄花芬, 黄晖, 等. 铝合金材料发展现状、趋势及展望[J]. 中国工程科学, 2020, 22(5): 68-75.
[4]SERSOUR Z, AMIROUCHE L. Effect of aging and annealing treatments on the microstructural behavior of some Al-Si based alloys[J]. Applied Mechanics and Materials, 2015, 775: 152-159.
[5]林枫, 陆文兴, 吴孟武. 热处理对压铸铝合金ZL102力学及导热性能的影响[J]. 铸造, 2022, 71(6): 683-688.
[6]金星, 高立新, 张大全. Al-Si合金腐蚀与防护的研究进展[J]. 全面腐蚀控制, 2010, 24(9): 12-16.
[7]郑弃非, 孙霜青, 温军国. 铝及铝合金在我国的大气腐蚀及其影响因素分析[J]. 腐蚀与防护, 2009, 30(6): 359-363.
[8]JIN G, LI S, LOU C S. The anode oxidation technics and the characteristics of the films of ZL101A Al-Si alloy[J]. Advanced Materials Research, 2014, 893: 566-569.
[9]SULLIVAN J P O, WOOD G C. The morphology and mechanism of formation of porous anodic films on aluminium[C]//Proceedings of the Royal Society A: Mathematical, Physical and Engineering Sciences (PRSA). 1970. London, England, UK. The Royal Society, 1970, 317(1531): 511-543.
[10]廖重重, 陈岁元. 铝阳极氧化膜及生长机理的研究进展[J]. 辽宁化工, 2012, 41(7): 699-701.
[11]王雨辰. 铝合金硫酸阳极氧化槽液的质量控制[J]. 科技创新与生产力, 2023, 44(8): 91-93.
[12]王英君, 刘洪雷, 王国军, 等. 新型高强稀土Al-Zn-Mg-Cu-Sc铝合金的阳极氧化及其抗腐蚀性能研究[J]. 中国腐蚀与防护学报, 2020, 40(2): 131-138.
[13]高崇, 江钟宇, 赵丕植, 等. 电流密度对5252铝合金阳极氧化膜性能的影响[J]. 电镀与环保, 2020, 40(3): 63-66.
[14]薛莹. 铝合金阳极氧化封孔工艺的探析[J]. 冶金与材料, 2021, 41(6): 129-130.
[15]张策, 张德忠, 潘学著, 等. 铝及铝合金阳极氧化膜封孔技术机理、应用及研究进展[J]. 电镀与涂饰, 2022, 41(18): 1305-1312.
[16]库尔班江·乌丝曼, 戴晓业, 史琳. 相变材料对储热系统换热速率的影响[J]. 东北大学学报(自然科学版), 2023, 44(9): 1292-1297.